    Magnetic influence on the frequency of the soft-phonon mode in the incipient ferroelectric EuTiO3

    Full text link
    The dielectric constant of the incipient ferroelectric EuTiO3_3 exhibits a sharp decrease at about 5.5K, at which temperature antiferromagnetic ordering of the Eu spins simultaneously appears, indicating coupling between the magnetism and dielectric properties. This may be attributed to the modification of the soft-phonon mode, T1μT_{1\mu}, which is the main contribution to the large dielectric constant, by the Eu spins(7μB\mu_B per Eu). By adding the coupling term between the magnetic and electrical subsystems as −g∑l∑<i,jql2Si→⋅Sj→ -g\sum\limits_l {\sum\limits_{< {i,j}} {q_l^2}} \overrightarrow {S_i} \cdot \overrightarrow {S_j} we show that the variation of the frequency of soft-phonon mode depends on the spin correlation between the nearest neighbors Eu spins and is substantially changed under a magnetic field.Comment: 13 pages, 4 figure

    Ordering Process and Its Hole Concentration Dependence of the Stripe Order in La{2-x}Sr{x}NiO{4}

    Full text link
    Ordering process of stripe order in La{2-x}Sr{x}NiO{4} with x being around 1/3 was investigated by neutron diffraction experiments. When the stripe order is formed at high temperature, incommensurability \epsilon of the stripe order has a tendency to show the value close to 1/3 for the samples with x at both sides of 1/3. With decreasing temperature, however, \epsilon becomes close to the value determined by the linear relation of \epsilon = n_h, where n_h is a hole concentration. This variation of the \epsilon strongly affects the character of the stripe order through the change of the carrier densities in stripes and antiferromagnetic domains.Comment: 5 pages, 3 figures, REVTeX, to be published in Phys. Rev.

    Photoemission Spectral Weight Transfer and Mass Renormalization in the Fermi-Liquid System La1−x_{1-x}Srx_xTiO3+y/2_{3+y/2}

    Full text link
    We have performed a photoemission study of La1−x_{1-x}Srx_xTiO3+y/2_{3+y/2} near the filling-control metal-insulator transition (MIT) as a function of hole doping. Mass renormalization deduced from the spectral weight and the width of the quasi-particle band around the chemical potential μ\mu is compared with that deduced from the electronic specific heat. The result implies that, near the MIT, band narrowing occurs strongly in the vicinity of μ\mu. Spectral weight transfer occurs from the coherent to the incoherent parts upon antiferromagnetic ordering, which we associate with the partial gap opening at μ\mu.Comment: 4 pages, 3 figure

    Universal charge transport of the Mn oxides in the high temperature limit

    Full text link
    We have found that various Mn oxides have the universal resistivity and thermopower in the high temperature limit. The resistivities and thermopowers of all the samples go toward constant values of 7±\pm1 mΩ\Omegacm and −79±-79\pm3 μ\muV/K, which are independent of carrier density and crystal structures. We propose that the electric conduction occurs in a highly localized way in the high temperature limit, where the exchange of entropy and charge occurs in the neighboring Mn3+^{3+} and Mn4+^{4+} ions.Comment: 4 pages, 4 eps figures, to be published in J. Appl. Phy

    Charge ordering and chemical potential shift in La2−x_{2-x}Srx_xNiO4_4 studied by photoemission spectroscopy

    Full text link
    We have studied the chemical potential shift in La2−x_{2-x}Srx_xNiO4_4 and the charge ordering transition in La1.67_{1.67}Sr0.33_{0.33}NiO4_4 by photoemission spectroscopy. The result shows a large (∼\sim 1 eV/hole) downward shift of the chemical potential with hole doping in the high-doping regime (δ≳\delta \gtrsim 0.33) while the shift is suppressed in the low-doping regime (δ≲\delta \lesssim 0.33). This suppression is attributed to a segregation of doped holes on a microscopic scale when the hole concentration is lower than δ≃1/3\delta \simeq 1/3. In the δ=1/3\delta = 1/3 sample, the photoemission intensity at the chemical potential vanishes below the charge ordering transition temperature TCO=T_{\rm CO}= 240 K.Comment: 5 pages, 4 figure

    Unconventional spin fluctuations in the hexagonal antiferromagnet YMnO3_3

    Full text link
    We used inelastic neutron scattering to show that well below its N\'{e}el temperature, TNT_{\rm N}, the two-dimensional (2D) XY nearly-triangular antiferromagnet YMnO3_{3} has a prominent {\it central peak} associated with 2D antiferromagnetic fluctuations with a characteristic life time of 0.55(5) ps, coexisting with the conventional long-lived spin-waves. Existence of the two time scales suggests competition between the N\'{e}el phase favored by weak interplane interactions, and the Kosterlitz-Thouless phase intrinsic to the 2D XY spin system.Comment: 4pages, 5figure

    Electronic Structure of Charge- and Spin-controlled Sr_{1-(x+y)}La_{x+y}Ti_{1-x}Cr_{x}O_{3}

    Get PDF
    We present the electronic structure of Sr_{1-(x+y)}La_{x+y}Ti_{1-x}Cr_{x}O_{3} investigated by high-resolution photoemission spectroscopy. In the vicinity of Fermi level, it was found that the electronic structure were composed of a Cr 3d local state with the t_{2g}^{3} configuration and a Ti 3d itinerant state. The energy levels of these Cr and Ti 3d states are well interpreted by the difference of the charge-transfer energy of both ions. The spectral weight of the Cr 3d state is completely proportional to the spin concentration x irrespective of the carrier concentration y, indicating that the spin density can be controlled by x as desired. In contrast, the spectral weight of the Ti 3d state is not proportional to y, depending on the amount of Cr doping.Comment: 4 pages, 3 figures. Accepted for publication in Phys. Rev. Let

    Stripe order at low temperatures in La{2-x}Sr{x}NiO4 for 1/3 < x < 1/2

    Full text link
    Stripe order in La{2-x}Sr{x}NiO4 beyond x = 1/3 was studied with neutron scattering technique. At low temperatures, all the samples exhibit hole stripe order. Incommensurability \epsilon of the stripe order is approximately linear in the hole concentration n_h = x + 2\delta up to x = 1/2, where \delta denotes the off-stoichiometry of oxygen atoms. The charge and spin ordering temperatures exhibit maxima at n_h = 1/3, and both decrease beyond n_h > 1/3. For 1/3 < n_h < 1/2, the stripe ordering consists of the mixture of the \epsilon = 1/3 stripe order and the n_h = 1/2 charge/spin order.Comment: REVTeX, 4 pages, 4 figure

    Charge dynamics of Ca_{2-x}Na_{x}CuO_{2}Cl_{2} as a correlated electron system with the ideal tetragonal lattice

    Full text link
    We report the reflectivity and the resistivity measurement of Ca_{2-x}Na_{x}CuO_{2}Cl_{2} (CNCOC), which has a single-CuO2-plane lattice with no orthorhombic distortion. The doping dependence of the in-plane optical conductivity spectra for CNCOC is qualitatively the same to those of other cuprates, but a slight difference between CNCOC and LSCO, i.e., the absence of the 1.5 eV peak in CNCOC, can be attributed to the smaller charge-stripe instability in CNCOC. The temperature dependence of the optical onductivity spectra of CNCOC has been analyzed both by the two-component model (Drude+Lorentzian) and by the one-component model (extended-Drude analysis). The latter analysis gives a universal trend of the scattering rate Gamma(omega) with doping. It was also found that Gamma(omega) shows a saturation behavior at high frequencies, whose origin is the same as that of resistivity saturation at high temperatures.Comment: 8 pages, 11 figures, to be published in Phys. Rev.
    • …